- Product category
-
Product name:ESD PC/ABS Compound
Product model:Anti Static Plastic
Product brand:INCHR
Processing customized:Dosage level 5~20 wt%
Product specification:Static Dissipative Compound
Product description:ESD C 2580 FR
Polycarbonate/ABS Alloy (PC/ABS)
ESD Protection
Electrically Conductive
Flame Retardant
PROPERTIES & AVERAGE VALUES OF INJECTION MOLDED SPECIMENS
PERMANENCEEnglish SI Metric ASTM
TESTSpecific Gravity 1.29 1.29 D 792 Molding Shrinkage 1/8 in (3.2 mm) section 0.0010 in/in 0.10 % D 955
MECHANICALImpact Strength, Izod notched 1/8 in (3.2 mm) section 1.0 ft-lbs/in 53 J/m D 256 unnotched 1/8 in (3.2 mm) section 6.0 ft-lbs/in 320 J/m D 4812 Tensile Strength 18000 psi 124 MPa D 638 Tensile Elongation 1.5 % 1.5 % D 638 Tensile Modulus 1.75 x 10^6 psi 12066 MPa D 638 Flexural Strength 25000 psi 172 MPa D 790 Flexural Modulus 1.50 x 10^6 psi 10342 MPa D 790
ELECTRICALVolume Resistivity < 1E0 ohm.cm < 1E0 ohm.cm D 257 Surface Resistivity < 1E4 ohm/sq < 1E4 ohm/sq D 257
ESD STM11.11
THERMALIgnition Resistance* Flammability** V-0 @ 1/16 in V-0 @ 1.5 mm D 3801 PROPERTY NOTES Data herein is typical and not to be construed as specifications.
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.* This rating is not intended to reflect hazards of this or any other material under actual fire conditions.
GENERAL PROCESSING FOR INJECTION MOLDINGEnglish SI Metric Injection Pressure 10000 - 15000 psi 69 - 103 MPa Melt Temperature 470 - 525 °F 243 - 274 °C Mold Temperature 125 - 200 °F 52 - 93 °C Drying 4 hrs @ 200 °F 4 hrs @ 93 °C Moisture Content 0.02 % 0.02 % Dew Point -20 °F -29 °C
PROCESSING NOTESDesiccant Type Dryer Required.
Next:ESD PPS Compound
Related products