Product name:ESD PPS Compound
Product model:Conductive Plastic Compound
Product brand:INCHR
Processing customized:Carbon Fiber Compound
Product specification:Surface Resistivity 10^3~10^5 Ohms
Product description:ESD C 1305
Polyphenylene Sulfide (PPS)
Glass Fiber
ESD Protection
Electrically Conductive plastic Compound
PROPERTIES & AVERAGE VALUES OF INJECTION MOLDED SPECIMENS
PERMANENCEEnglish SI Metric ASTM
TESTSpecific Gravity 1.65 1.65 D 792 Molding Shrinkage 1/8 in (3.2 mm) section 0.0020 - 0.0030 in/in 0.20 - 0.30 % D 955
MECHANICALImpact Strength, Izod notched 1/8 in (3.2 mm) section 0.9 ft-lbs/in 48 J/m D 256 unnotched 1/8 in (3.2 mm) section 2.5 ft-lbs/in 133 J/m D 4812 Tensile Strength 12500 psi 86 MPa D 638 Tensile Elongation 0.5 - 1.5 % 0.5 - 1.5 % D 638 Tensile Modulus 1.90 x 10^6 psi 13100 MPa D 638 Flexural Strength 17500 psi 121 MPa D 790 Flexural Modulus 1.90 x 10^6 psi 13100 MPa D 790
ELECTRICALVolume Resistivity < 1E3 ohm.cm < 1E3 ohm.cm D 257 Surface Resistivity < 1E6 ohm/sq < 1E6 ohm/sq D 257
ESD STM11.11Surface Resistance < 1E5 ohm < 1E5 ohm ESD STM11.11 Static Decay MIL-PRF-81705D, 5kV to 50 V, 12% RH < 2.00 s < 2.00 s FTMS101C
4046.1PROPERTY NOTES Data herein is typical and not to be construed as specifications.
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.
GENERAL PROCESSING FOR INJECTION MOLDINGEnglish SI Metric Injection Pressure 10000 - 15000 psi 69 - 103 MPa Melt Temperature 585 - 625 °F 307 - 329 °C Mold Temperature 275 - 350 °F 135 - 177 °C Drying 6 hrs @ 300 °F 6 hrs @ 149 °C Moisture Content 0.04 % 0.04 %
PROCESSING NOTES